plastic screws differ from metal in one fundamental way: they can be made in any colour, and colour is often what the customer is buying. Housings are black, medical equipment off-white, PV junction boxes light grey - and a batch-to-batch colour shift is painfully obvious once parts sit on the same machine. Worse are black spots, flow marks and silver streaks, which do not affect strength but decide acceptance. We manage colour and appearance as distinct quality characteristics.

Why colour variation bites harder on plastics

Metal appearance is set by plating or polishing and stays essentially constant. Plastic colour comes from pigment dispersed in a matrix and is shifted by resin lot, masterbatch ratio, melt temperature, screw residence time and mould temperature; any drift shows up as colour. Add the matt or semi-matt surfaces typical of these parts, where the same numerical difference looks quite different, and the sensitivity of the eye to adjacent parts, and judging colour under one light and one background stops being optional.

Colour approval as a shared reference

Before series production, make a standard colour plaque signed by both customer and supplier, recording colour code, material, surface finish and gloss. Keep copies on both sides so there is no later dispute about what was agreed. Approve a tolerance at the same time: for example visual comparison against the plaque not below a stated grey scale rating, or an instrumented colour difference limit. Signing a plaque without a tolerance turns into unlimited nitpicking or unlimited leniency, and both end in argument.

Masterbatch dosing and mixing

The most common source of colour shift is not moulding but dosing. Hand-weighed masterbatch drifts by a percent, which is visible on light parts, and uneven mixing leaves cloudy patches. Use a metering blender, fix one masterbatch supplier per grade, record ratio and mixing time per batch, and purge thoroughly on colour changes. Going from dark to light is the hard direction, because screw and barrel residue resists cleaning; transition material is usually needed and that loss belongs in the quotation.

How moulding parameters shift colour

High melt temperature degrades some pigments or changes their tone; low temperature disperses poorly and leaves streaks. Long residence time accumulates heat history and yellows light parts. Mould temperature changes crystallinity, and in crystalline materials both gloss and hue move with it. Colour adjustment therefore cannot be a temperature tweak at the machine: lock melt temperature, mould temperature, injection speed and packing as controlled parameters with permitted ranges on the process card, and compare a small sample before deciding a new lot needs re-setting.

Batch comparison: criteria and method

Sample at fixed intervals and compare with the plaque in a standard light booth whose colour temperature is close to the customer's inspection environment, rather than judging under one light only. Where instruments are available, use a spectrophotometer and record deviation in lightness, hue and saturation, which localises the cause better than a single number. Split criteria between visible and hidden surfaces: tight on faces the user sees, relaxed where the part is buried after assembly, so appearance is protected without scrapping usable parts.

Black spots, flow marks and silver streaks

Black spots come from carbonised residue in the barrel or airborne dust; they appear randomly, are small, and contrast strongly, especially on light parts. Flow marks are ripples from the melt front cooling in the cavity, typically opposite the gate. Silver streaks are moisture or volatiles expanding in the melt, which points to inadequate drying. The three have entirely different causes, so raising temperature or pressure to suppress them usually trades one defect for another.

Packing and the risk of mixed parts

For appearance parts the real danger is not a single defect but mixed parts. Colours and sizes look alike, the customer's line cannot separate them, and the whole carton comes back. Controls are separate packing per colour and size, clearing the area at changeover, never staging two colours in the packing zone at once, and labelling with colour code and batch. Bulk shipments need a lined bag and a seal, since transit abrasion marks are judged as appearance defects just the same.

Complaint traceability and improvement

On a colour or appearance complaint, first obtain the physical part and batch number from the customer and compare with the retention sample, separating an individual deviation from a whole-batch shift. Batch shifts usually trace to resin or masterbatch change; individual deviations to process fluctuation or mixed parts. Retention sampling is the foundation, kept beyond the customer's acceptance window. We retain samples per batch with colour code, masterbatch lot and moulding parameters, so a dispute can be resolved the same day.