RENY Screws: Non-Magnetic Behaviour and MRI Compatibility Verified

Home-News-RENY Screws: Non-Magnetic Behaviour and MRI Compatibility Verified

RENY Screws: Non-Magnetic Behaviour and MRI Compatibility Verified

RENY Screws: Non-Magnetic Behaviour and MRI Compatibility Verified

Around an MRI scanner there is an often underestimated restriction: any ferromagnetic material can be attracted by the main field, become a projectile, or disturb field homogeneity inside the imaging volume and create artefacts. Fasteners on housings, patient table accessories and coil mounts are therefore frequently specified non-magnetic. RENY, a glass-reinforced MXD6 polyamide, contains no ferromagnetic elements and is widely used for exactly this. Non-magnetic is not zero susceptibility, though, nor unit-level compatibility.

What non-magnetic actually means

Materials divide magnetically into ferromagnetic, ferrimagnetic, paramagnetic and diamagnetic. Iron, cobalt, nickel and their alloys are ferromagnetic, strongly attracted and the first thing to exclude from an MRI environment. Many stainless grades such as 304 can carry weak magnetism after working, and 316 is weaker but not absolutely zero. Plastics, ceramics, aluminium and copper are paramagnetic or diamagnetic with very low susceptibility, effectively non-magnetic in engineering terms. RENY belongs here: it is not attracted and does not noticeably disturb the field.

Susceptibility and image artefacts

Non-magnetic does not mean no imaging effect. A susceptibility difference between material and tissue creates a local field gradient at the interface, producing distortion and signal loss - artefact. The larger the difference and the closer the part to the imaging volume, the more visible it becomes. Plastics sit close to water in susceptibility and are theoretically far gentler than metals, but glass content, filler type and part volume still matter. Where a part lies in the field of view near sensitive sequences, verify by actual scanning rather than material class alone.

Comparison with alternative materials

Common alternatives are PPS, peek, ceramics and titanium. PPS offers better chemical and thermal resistance with slightly lower strength; peek performs excellently but costs more; ceramics excel in insulation and wear resistance but are brittle and hard to machine; titanium is strongest, paramagnetic and generally acceptable near MRI, though it still produces some artefact. The choice trades strength, temperature, cost and imaging requirements. RENY sits as a well-balanced non-magnetic option with good machinability and molding behaviour.

Glass content and its effect on inspection

RENY derives strength from glass fibre; higher content brings stiffness and lower shrinkage but also brittleness and faster tool wear. For non-magnetic purposes the fibre is a silicate material with no ferromagnetic component, so reinforcement does not compromise the property. Watch colourants, however: some dark or special shades use inorganic pigments, and certain pigments contain iron oxides that introduce weak magnetism. Where colour is specified on an MRI part, confirm the colour code and composition at material approval.

From a magnet to susceptibility measurement

The crudest check is a strong magnet: anything attracted fails, which is simple but only catches clearly ferromagnetic parts. A step up uses a gaussmeter or fluxmeter to measure response in a field and compare against a reference part from the same family. For demanding work, a vibrating sample magnetometer gives quantitative susceptibility. Whichever method, contamination matters: iron dust from machining or packaging makes a non-magnetic part behave magnetically, so clean before testing and never store with carbon steel.

Unit-level MRI compatibility testing

A non-magnetic part does not guarantee a compatible unit. Three tests are typical: projectile force, confirming the part is not attracted in a strong field; heating, confirming no significant temperature rise under radio frequency; and imaging, confirming no visible artefact with the part present. All three depend on mass, volume, position and fixing method. If a customer specifies material only and skips unit testing, the supplier should state the boundary of responsibility and provide susceptibility data and cleanliness records for the customer's assessment.

Why complaints actually happen

Genuine out-of-spec magnetism is rare in complaints. Three other causes dominate: carbon steel screws mixed in at assembly, visually hard to tell apart; iron dust on the surface or shipping in the same box as carbon steel; and artefacts blamed on fasteners when the real source is nearby metal structure. Investigate on site: screen parts individually with a magnet, inspect packaging and tote boxes, and review the surrounding structure. We run MRI parts on dedicated lines with separate packing and ship material certificates with magnetic screening records.

Closing: specify the test, not just the material

For MRI-adjacent equipment, the specification should state the acceptance method as well as the material: magnet screening of every part, susceptibility data where imaging is critical, dedicated packing, and a clear division of responsibility for unit-level projectile, heating and artefact testing. RENY is a sound choice for structural and housing fastening in these environments, provided colourants and contamination are controlled. We produce such parts on dedicated lines with separate packing and full material documentation to keep on-site misdiagnosis out of the picture.